Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity at 100°C (212°F) | 19.3 cSt | 19.3 cSt | |
ChevronTexaco Quenchtex® MM Texaco Quenchtex oils deliver value through:Controlled cooling of metals — Combines the high initial quenching speed of water with slow final quenching speed of oil.Safety — High flash point and f.. |
|||
Kinematic Viscosity at 100°C (212°F) | 19.3 cSt | 19.3 cSt | ASTM D445 |
ChevronTexaco RPM® SAE 50 Heavy Duty Motor Oil Features: Chevron RPM Heavy Duty Motor Oils are premium quality, mixed fleet motor oils meeting the performance requirements of all four-stroke gasoline engines and all naturally aspirated, turbocha.. |