Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Kinematic Viscosity at 100°C (212°F) 30.4 cSt
30.4 cSt
ASTM D445
ExxonMobil Teresstic 460
TERESSTIC is the brand name for a line of long-service-life lubricating oils that have ranked for over five decades among the finest products of their kind. Continually improved over the years, TERE..
Kinematic Viscosity at 100°C (212°F) 30.4 cSt
30.4 cSt
ASTM D445
ChevronTexaco ISO 460 Cylinder Oil W
FeaturesChevron Cylinder Oils W are designed to meet the needs of emulsifying cylinder oils.Chevron Cylinder Oils W provide excellent metal wettability. The combination of oil emulsibility and metal..
Kinematic Viscosity at 100°C (212°F) 30.4 cSt
30.4 cSt
ChevronTexaco Vanguard® 460
Texaco Vanguard oils deliver value through:Excellent metal wettability and high film strength for any moisture condition.Versatility — Three viscosity grades available to cover the range of steam p..
Kinematic Viscosity at 100°C (212°F) 30.4 cSt
30.4 cSt
ASTM D445
ExxonMobil Teresstic 460
TERESSTIC is the brand name for a line of long-service-life lubricating oils that have ranked for over five decades among the finest products of their kind. Continually improved over the years, TERE..
Kinematic Viscosity at 100°C (212°F) 30.4 cSt
30.4 cSt
ConocoPhillips Hydroclear® 2500 Industrial Oil
Description: Conoco Hydroclear Industrial Oil is a high-quality, general-purpose industrial lubricant formulated from premium Conoco hydrocracked base stocks. Hydroclear Industrial Oil is recommende..