Polymer Property : Kinematic Viscosity at 100°C (212°F) = 4.0 cSt Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Kinematic Viscosity at 100°C (212°F) 4.0 cSt
4.0 cSt
Base Oil; ASTM D445
Nye Lubricants DHL-400 Oil
Information provided by Nye Lubricants.
Kinematic Viscosity at 100°C (212°F) 4.0 cSt
4.0 cSt
Base Oil; ASTM D445
Nye Lubricants UniFlor 8310 (472) (UF) Synthetic Oil
Information provided by Nye Lubricants.
Kinematic Viscosity at 100°C (212°F) 4.0 cSt
4.0 cSt
Base Oil; ASTM D445
Nye Lubricants UniFlor 8311 (833-1) (UF) Synthetic Oil
Information provided by Nye Lubricants.
Kinematic Viscosity at 100°C (212°F) 4.0 cSt
4.0 cSt
Base Oil; ASTM D445
Nye Lubricants 833Z-1 (FG) Synthetic Oil
Information provided by Nye Lubricants.
Kinematic Viscosity at 100°C (212°F) 4.0 cSt
4.0 cSt
ExxonMobil Mobil Turbo 24
Mobil Turbo 284 gas turbine lubricant is a combination of a highly stable synthetic base fluid and a unique chemical additive package. The result is a product having superior thermal and oxidation ..
Kinematic Viscosity at 100°C (212°F) 4.0 cSt
4.0 cSt
ASTM D445, DIN 51 561
Chesterton 601 Chain Drive Pin & Bushing Lubricant
Description: Chesterton® 601 Chain Drive Pin & Bushing Lubricant is and has been the premium quality light lubricant of choice in industry for over thirty years. This superior lubricant was special..
Kinematic Viscosity at 100°C (212°F) 4.0 cSt
4.0 cSt
ASTM D445
ChevronTexaco 100R Neutral Oil
FeaturesChevron Neutral Oils are all-hydroprocessed, highly refined API Group II paraffinic base stocks. Their extremely low sulfur, nitrogen, and aromatic content give them excellent thermal and o..
Kinematic Viscosity at 100°C (212°F) 4.0 cSt
4.0 cSt
ChevronTexaco Canopus® 19
Texaco Canopus oils deliver value through:High resistance to forming emulsions due to excellent water separating characteristics.Long lubricant life provided by outstanding stability.Good lubricant ..
Kinematic Viscosity at 100°C (212°F) 4.0 cSt
4.0 cSt
ASTM D445
ChevronTexaco CP Grease
FeaturesChevron CP Grease is a corrosion preventive grease.It is manufactured with a special low viscosity, low pour point base oil, a lithium thickener, and rust and oxidation inhibitors. It is lig..
Kinematic Viscosity at 100°C (212°F) 4.0 cSt
4.0 cSt
ASTM D445
ChevronTexaco ISO 22 CP Oil
FeaturesChevron CP Oil is used for both cotton picker spindle lubrication and as a corrosion (rust) preventative on steel materials in the steel industry.It is manufactured form medium viscosity ind..
Kinematic Viscosity at 100°C (212°F) 4.0 cSt
4.0 cSt
See Note 3.
ChevronTexaco MCP Grease L NLGI Grade 00
Typical test data are average values only. Minor variations which do not affect product performance are to be expected in normal manufacturing.Notes:Minimum operating temperature is the lowest tempe..
Kinematic Viscosity at 100°C (212°F) 4.0 cSt
4.0 cSt
ASTM D445
ChevronTexaco Mechanism LPS® ISO 15 Hydraulic Oil
Chevron Mechanism LPS Hydraulic Oils are highly refined, paraffinic oils containing oxidation and rust inhibitors, and special antiwear additives to extend the life of hydraulic pumps and motor part..
Kinematic Viscosity at 100°C (212°F) 4.0 cSt
4.0 cSt
ChevronTexaco Quenchtex® A
Texaco Quenchtex oils deliver value through:Controlled cooling of metals — Combines the high initial quenching speed of water with slow final quenching speed of oil.Safety — High flash point and f..
Kinematic Viscosity at 100°C (212°F) 4.0 cSt
4.0 cSt
ChevronTexaco Quenchtex® B
Texaco Quenchtex oils deliver value through:Controlled cooling of metals — Combines the high initial quenching speed of water with slow final quenching speed of oil.Safety — High flash point and f..
Kinematic Viscosity at 100°C (212°F) 4.0 cSt
4.0 cSt
ChevronTexaco Rando® HDZ 15
Texaco Rando HDZ oils deliver value through:High oxidation stability — Longer service life than attainable with conventional lubricants used in high pressure service.Protection against rust and cor..
Kinematic Viscosity at 100°C (212°F) 4.0 cSt
4.0 cSt
ASTM D445
ChevronTexaco Rykon® ISO 15 Premium Oil
FeaturesChevron Rykon Premium Oils are designed to give maximum protection to hydraulic pumps.They are formulated with ISOSYN® base stocks incorporating antiwear additives, oxidation and corrosion ..
Kinematic Viscosity at 100°C (212°F) 4.0 cSt
4.0 cSt
ExxonMobil Mobil Turbo 24
Mobil Turbo 284 gas turbine lubricant is a combination of a highly stable synthetic base fluid and a unique chemical additive package. The result is a product having superior thermal and oxidation ..
Kinematic Viscosity at 100°C (212°F) 4.0 cSt
4.0 cSt
ASTM D445
ExxonMobil Mobil Velocite 10
The Mobil Velocite Oil Numbered Series oils are premium performance products primarily designed for the lubrication of high-speed spindles in machine tools. They are also used in some critical hydra..
Kinematic Viscosity at 100°C (212°F) 4.0 cSt
4.0 cSt
ASTM D-445
ConocoPhillips ANDEROL® FGC 5 Fluid, Synthetic Mechanical Seal Fluid ISO 22
Description: ANDEROL FGC 5 Mechanical Seal Fluid is a synthetic hydrocarbon (PAO) based lubricant. FGC 5 Fluid meets the former H-1 approval requirements of the USDA where incidental food contact ca..
Kinematic Viscosity at 100°C (212°F) 4.0 cSt
4.0 cSt
ASTM D-445
ConocoPhillips ANDEROL® FGH 22 Synthetic Food Grade Hydraulic Fluid, ISO 22
Description: ANDEROL FGH Series Hydraulic Fluids are made from synthetic hydrocarbons (PAO) and special additive packages which allow them to meet the former H-1 approval requirements of the USDA wh..
Kinematic Viscosity at 100°C (212°F) 4.0 cSt
4.0 cSt
Base Oil; ASTM D445
Nye Lubricants 799 (RL) Synthetic Oil
Information provided by Nye Lubricants.
Kinematic Viscosity at 100°C (212°F) 4.0 cSt
4.0 cSt
ASTM D445
ExxonMobil Mobil Velocite 10
The Mobil Velocite Oil Numbered Series oils are premium performance products primarily designed for the lubrication of high-speed spindles in machine tools. They are also used in some critical hydra..