Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity at 100°C (212°F) | 41 cSt | 41 cSt | ASTM D445 |
Solvay Specialty Polymers FOMBLIN® W800 PFPE Lubricant Fomblin® PFPE fluorinated lubricants are used when harsh chemical environments, high temperatures or wide working-temperature ranges are encountered.Information provided by Solvay Solexis, Inc. |