Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity at 100°C (212°F) | 6.5 cSt | 6.5 cSt | ASTM D445 |
ExxonMobil Mobil Zerice 68 S Oil Mobil Zerice S Oils are premium quality synthetic refrigeration compressor lubricants. Based on alkyl benzenes, which due to their nature, have superior miscibility with hydrochlorofluorocarbon (R2.. |
|||
Kinematic Viscosity at 100°C (212°F) | 6.5 cSt | 6.5 cSt | ASTM D445 |
ChevronTexaco 220R Neutral Oil FeaturesChevron Neutral Oils are all-hydroprocessed, highly refined API Group II paraffinic base stocks. Their extremely low sulfur, nitrogen, and aromatic content give them excellent thermal and o.. |
|||
Kinematic Viscosity at 100°C (212°F) | 6.5 cSt | 6.5 cSt | |
ChevronTexaco 46 AW Hydraulic Oil Texaco AW Hydraulic Oils deliver value through:High oxidation stability — Longer service life than with conventional lubricants in high pressure service.Rust and corrosion protection — Gives excel.. |
|||
Kinematic Viscosity at 100°C (212°F) | 6.5 cSt | 6.5 cSt | ASTM D445 |
ChevronTexaco Bright-Cut® NM Metal Working Fluid FeaturesChevron Bright-Cut Metalworking Fluids are a complete line of chlorine-free cutting oils that offer benefits not found in conventional cutting oils.The unique synthetic antiweld components .. |
|||
Kinematic Viscosity at 100°C (212°F) | 6.5 cSt | 6.5 cSt | ASTM D445 |
ChevronTexaco ISO 46 AIO FeaturesChevron AIO (Chevron Authentic Industrial Oils) provide rust protection, oxidation inhibition, and foam suppression.Chevron AIO are good quality lubricants for any application not requiring .. |
|||
Kinematic Viscosity at 100°C (212°F) | 6.5 cSt | 6.5 cSt | ASTM D445 |
ChevronTexaco ISO 46 Hydraulic Oil AW FeaturesChevron Hydraulic Oils AW are designed to give excellent hydraulic pump protection. They are formulated with refined paraffinic base oils. They provide excellent antiwear protection, oxidati.. |
|||
Kinematic Viscosity at 100°C (212°F) | 6.5 cSt | 6.5 cSt | ASTM D445 |
ChevronTexaco ISO 46 Industrial Oil EP FeaturesChevron Industrial Oils EP are multipurpose oils for industrial service.Chevron Industrial Oils EP are designed to help minimize wear in all types of plant lubrication and also provide long .. |
|||
Kinematic Viscosity at 100°C (212°F) | 6.5 cSt | 6.5 cSt | ASTM D445 |
ChevronTexaco ParaLux® 2401R Process Oil FeaturesPARALUX is produced using an all-hydroprocessing route which transforms the molecular structure of undesirable aromatics into highly desirable saturates. This produces a process oil with sup.. |
|||
Kinematic Viscosity at 100°C (212°F) | 6.5 cSt | 6.5 cSt | ASTM D445 |
ChevronTexaco ParaLux™ 2401 Paraffinic Process Oil FeaturesPARALUX is produced using an all-hydroprocessing route which transforms the molecular structure of undesirable aromatics into highly desirable saturates. This produces a process oil with sup.. |
|||
Kinematic Viscosity at 100°C (212°F) | 6.5 cSt | 6.5 cSt | ASTM D445 |
ChevronTexaco Regal® 46 R&O Texaco Regal R&O oils deliver value through:Prolonged oil service life — Excellent oxidation stability provided by the multi-component inhibitor system resists oil breakdown during exposure to high.. |
|||
Kinematic Viscosity at 100°C (212°F) | 6.5 cSt | 6.5 cSt | ASTM D445 |
ChevronTexaco Rykon® ISO 46 Oil AW FeaturesChevron Rykon Oils AW are designed to give maximum hydraulic pump protection.Chevron Rykon Oils AW are formulated with ISOSYN® base stocks.They provide excellent antiwear protection, oxidat.. |
|||
Kinematic Viscosity at 100°C (212°F) | 6.5 cSt | 6.5 cSt | ASTM D445 |
ChevronTexaco Vistac® ISO 46 Rock Drill Oil FeaturesChevron Rock Drill Oils Vistac are designed to give maximum protection to percussion rock drills.They are formulated from highly refined, high viscosity index, paraffinic base stocks and add.. |
|||
Kinematic Viscosity at 100°C (212°F) | 6.5 cSt | 6.5 cSt | ASTM D445 |
ExxonMobil Mobil Zerice 68 S Oil Mobil Zerice S Oils are premium quality synthetic refrigeration compressor lubricants. Based on alkyl benzenes, which due to their nature, have superior miscibility with hydrochlorofluorocarbon (R2.. |
|||
Kinematic Viscosity at 100°C (212°F) | 6.5 cSt | 6.5 cSt | |
ConocoPhillips C-3 Hydraulic Transmission Fluid, Type C-3 Description: Conoco Hydraulic Transmission Fluid, Type C-3 is a heavy-duty, low viscosity fluid for mobile hydraulic systems, torque converters and automatic transmissions. Use it in Allison powersh.. |
|||
Kinematic Viscosity at 100°C (212°F) | 6.5 cSt | 6.5 cSt | |
ConocoPhillips Hydroclear Diamond Class® 32/46 Rotary Compressor Fluid Description: Conoco Hydroclear Diamond Class Rotary Compressor Fluids are designed to lubricate rotary screw compressors operating in air compression service. These semisynthetic products combine hi.. |
|||
Kinematic Viscosity at 100°C (212°F) | 6.5 cSt | 6.5 cSt | |
ConocoPhillips Hydroclear® 10W Fluid 10W Description: Conoco Hydroclear PowerDrive Fluid meets the stringent performance requirements of powershift transmissions, final drives, and wet-disc brakes typically found in equipment manufactured .. |
|||
Kinematic Viscosity at 100°C (212°F) | 6.5 cSt | 6.5 cSt | |
ChevronTexaco Aries® 46 Texaco Aries lubricants deliver value through:Long equipment life — Extreme pressure performance withstands heavy shock loads typical of rock drill service, protecting the equipment against rapid w.. |
|||
Kinematic Viscosity at 100°C (212°F) | 6.5 cSt | 6.5 cSt | Base Oil; ASTM D445 |
Chesterton 633 SXCM Synthetic, Extreme Pressure & Corrosion Resistant Grease-with Moly Description: Chesterton® 633 Synthetic Extreme Pressure & Corrosion Resistant Grease with Moly is the one grease to use for the most demanding lubricating needs. It is a multi-purpose workhorse wit.. |
|||
Kinematic Viscosity at 100°C (212°F) | 6.5 cSt | 6.5 cSt | |
ChevronTexaco Rando® HD 46 Texaco Rando HD oils deliver value through:Longer equipment life — Special antiwear additive package reduces wear by protecting surfaces when load causes breakdown of the lubricant film.Reduced dow.. |