Kinematic Viscosity at 100°C (212°F) 65 cSt
65 cSt
ASTM D445
ExxonMobil SpectraSyn Elite™ 65 Metallocene Polyalphaolefin (mPAO) Fluid
Product Description: SpectraSyn ™ metallocene Polyalphaolefin (mPAO) basestock is an advanced high viscosity (Hi-Vis) Polyalphaolefin (PAO). SpectraSyn ™ mPAO utilized metallocene catalyst technol..