Polymer Property : Kinematic Viscosity at 100°C (212°F) = 7.0 cSt Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Kinematic Viscosity at 100°C (212°F) 7.0 cSt
7.0 cSt
Base Oil; ASTM D445
Nye Lubricants 951 (RL) Synthetic Oil
Information provided by Nye Lubricants.
Kinematic Viscosity at 100°C (212°F) 7.0 cSt

@Temperature 100 °C
7.0 cSt

@Temperature 212 °F
ASTM D445
PolyOne Synplast™ NOTM-E Tri (n-octyl) Trimellitate
Linear trimellitate esterContains 0.10-0.15 wt% 1,1,3-Tris (2-methyl-4hydroxy-5-t-butyl phenyl) butane antioxidantInformation provided by PolyOne
Kinematic Viscosity at 100°C (212°F) 7.0 cSt

@Temperature 100 °C
7.0 cSt

@Temperature 212 °F
ASTM D445
PolyOne Synplast™ NOTM-PPC Tri (n-octyl) Trimellitate
CPSIA HR 4040 Compliant Linear trimellitate esterContains 0.10-0.15 wt% 1,1,3-Tris (2-methyl-4hydroxy-5-t-butyl phenyl) butane antioxidantInformation provided by PolyOne
Kinematic Viscosity at 100°C (212°F) 7.0 cSt
7.0 cSt
Base Oil; ASTM D445
Nye Lubricants 782G (NG) Synthetic Oil
Information provided by Nye Lubricants.
Kinematic Viscosity at 100°C (212°F) 7.0 cSt
7.0 cSt
ASTM D445
ChevronTexaco 7R Unconventional Base Oil
FeaturesChevron Unconventional Base Oils (UCBOs) are all hydroprocessed, highly refined paraffinic base oils of exceptional performance and purity.Relative to conventional hydroprocessed and solvent..
Kinematic Viscosity at 100°C (212°F) 7.0 cSt
7.0 cSt
ASTM D445
ChevronTexaco RPM® SAE 10W Heavy Duty Motor Oil
Features: Chevron RPM Heavy Duty Motor Oils are premium quality, mixed fleet motor oils meeting the performance requirements of all four-stroke gasoline engines and all naturally aspirated, turbocha..
Kinematic Viscosity at 100°C (212°F) 7.0 cSt
7.0 cSt
ChevronTexaco Starguide™ ISO 46
Texaco Starguide oils deliver value through:Cleaner cutting — Reduce excessive drag that slows cutting.Exceptional performance for low water and low oil consumption saw systems.Excellent low temper..
Kinematic Viscosity at 100°C (212°F) 7.0 cSt
7.0 cSt
ASTM D445
ChevronTexaco Torque Fluid
Chevron Torque Fluid is a high performance hydraulic fluid designed for use in transmissions and hydraulic systems requiring a fluid meeting the Allison C4 specificationIt is manufactured using high..
Kinematic Viscosity at 100°C (212°F) 7.0 cSt
7.0 cSt
ASTM D-445
ConocoPhillips ANDEROL® 783-0 Series Synthetic Food Grade Greases, NLGI Grade 0
Description: ANDEROL 783 Series Greases are made from synthetic hydrocarbons (PAO) and an aluminum complex soap thickener, allowing for a wide range of operating temperatures. The 783 Series Greases..
Kinematic Viscosity at 100°C (212°F) 7.0 cSt
7.0 cSt
ASTM D-445
ConocoPhillips ANDEROL® 783-00 Series Synthetic Food Grade Greases, NLGI Grade 00
Description: ANDEROL 783 Series Greases are made from synthetic hydrocarbons (PAO) and an aluminum complex soap thickener, allowing for a wide range of operating temperatures. The 783 Series Greases..
Kinematic Viscosity at 100°C (212°F) 7.0 cSt
7.0 cSt
ASTM D-445
ConocoPhillips ANDEROL® 783-1 Series Synthetic Food Grade Greases, NLGI Grade 1
Description: ANDEROL 783 Series Greases are made from synthetic hydrocarbons (PAO) and an aluminum complex soap thickener, allowing for a wide range of operating temperatures. The 783 Series Greases..
Kinematic Viscosity at 100°C (212°F) 7.0 cSt
7.0 cSt
ASTM D445
ChevronTexaco Clarity® ISO 46 Saw Guide Oil
FeaturesChevron Clarity Saw Guide Oils are designed to promote longer saw guide and saw blade life in thin kerf saw equipment, when operating in severe service and reduced cooling water modes.Chevro..