Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 0.35 cP @Temperature 121 °C |
0.35 cP @Temperature 250 °F |
|
Paratherm Corporation Paratherm™ CR Heat Transfer Fluid Paratherm CR® heat transfer fluid is a blend of synthetic components formulated to provide superior cooling performance in closed-loop heat-transfer systems operating down to -88°C (-127°F) yet i.. |
|||
Viscosity | 0.35 cP @Temperature 200 °C |
0.35 cP @Temperature 392 °F |
|
Solvay Chemicals Glycerol alpha monochlorohydrin Viscous liquid used as chemical intermediate.EINECS Number: 202-492-4/CAS Number: 96-24-2/UN number: 2689Information provided by Solvay |