Physical Properties Metric English Comments
Viscosity 0.53 cP

@Temperature 238 °C
0.53 cP

@Temperature 460 °F
Paratherm Corporation Paratherm™ GLT™ Heat Transfer Fluid
Paratherm GLT™ Heat Transfer Fluid is an alkylated aromatic based heat transfer fluid formulated for closed loop liquid phase heating systems to 550°F using fired heaters and to 575°F in waste-he..
Viscosity 0.53 cP

@Temperature 0.000 °C
0.53 cP

@Temperature 32.0 °F
Dynamic
Solvay Chemicals A50 Methylene chloride
Thanks to its specific characteristics, especially high solvent power, it is used where a high-grade economic solvent is required, because it successfully dissolves many organic compounds. Its high ..
Viscosity 0.53 cP

@Temperature 0.000 °C
0.53 cP

@Temperature 32.0 °F
Dynamic
Solvay Chemicals E2000 Methylene chloride
Thanks to its specific characteristics, especially high solvent power, it is used where a high-grade economic solvent is required, because it successfully dissolves many organic compounds. Its high ..