Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 200000 - 1.00e+6 cP @Temperature 190 - 190 °C |
200000 - 1.00e+6 cP @Temperature 374 - 374 °F |
Average value: 700000 cP Grade Count:5 |
Overview of materials for EMAAA Terpolymer This property data is a summary of similar materials in the MatWeb database for the category "EMAAA Terpolymer". Each property range of values reported is minimum and maximum values of appropriate M.. |
|||
Viscosity | 200000 - 1.00e+6 cP @Shear Rate 50.0 - 50.0 1/s |
200000 - 1.00e+6 cP @Shear Rate 50.0 - 50.0 1/s |
Average value: 700000 cP Grade Count:5 |
Overview of materials for EMAAA Terpolymer This property data is a summary of similar materials in the MatWeb database for the category "EMAAA Terpolymer". Each property range of values reported is minimum and maximum values of appropriate M.. |