Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 1.15e+6 cP @Shear Rate 1.00 1/s, Temperature 230 °C |
1.15e+6 cP @Shear Rate 1.00 1/s, Temperature 446 °F |
|
DSM Arnite® TM4 440 (PBT+PET)-MD20 20% Mineral Reinforced |