Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 1.43 cP @Temperature 5.00 °C |
1.43 cP @Temperature 41.0 °F |
|
Solvay Chemicals Epichlorohydrin Epichlorohydrin is a chemical intermediate, mainly dedicated to the manufacturing of epoxy resins used in Paints & coatings, Composites, Adhesives and Electronics. It is also used in non-epoxy appli.. |
|||
Viscosity | 1.43 cP @Temperature 150 °C |
1.43 cP @Temperature 302 °F |
|
Solvay Chemicals Glycerol alpha monochlorohydrin Viscous liquid used as chemical intermediate.EINECS Number: 202-492-4/CAS Number: 96-24-2/UN number: 2689Information provided by Solvay |