Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 115740 cP @Shear Rate 5000 1/s, Temperature 240 °C |
115740 cP @Shear Rate 5000 1/s, Temperature 464 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® HTR4275 BK316 Polyester Elastomer TPC-ET
(Unverified Data**) 55 Shore D High Viscosity Polyester Elastomer with Good Heat Ageing Protection Developed for Blow Molding Hytrel HTR4275 BK316 is designed for blow molding or processing techniques requiring high me.. |