Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 120 cP @Shear Rate 100 1/s, Temperature 280 °C |
120 cP @Shear Rate 100 1/s, Temperature 536 °F |
|
Solvay TECHNYL® A 218 V25 Black 21 N PA66, 25% glass fiber, DRY Description: TECHNYL® A 218 V25 is a polyamide 66, reinforced with 25% of glass fiber, heat stabilized, for injection molding. This product is available in natural and black colors.Benefits: The .. |
|||
Viscosity | 120 cP @Shear Rate 100 1/s, Temperature 290 °C |
120 cP @Shear Rate 100 1/s, Temperature 554 °F |
|
Solvay TECHNYL® A 218 V25 Black 21 N PA66, 25% glass fiber, DRY Description: TECHNYL® A 218 V25 is a polyamide 66, reinforced with 25% of glass fiber, heat stabilized, for injection molding. This product is available in natural and black colors.Benefits: The .. |
|||
Viscosity | 120 cP @Shear Rate 100 1/s, Temperature 300 °C |
120 cP @Shear Rate 100 1/s, Temperature 572 °F |
|
Solvay TECHNYL® A 218 V25 Black 21 N PA66, 25% glass fiber, DRY Description: TECHNYL® A 218 V25 is a polyamide 66, reinforced with 25% of glass fiber, heat stabilized, for injection molding. This product is available in natural and black colors.Benefits: The .. |
|||
Viscosity | 120 cP @Shear Rate 10.0 1/s, Temperature 300 °C |
120 cP @Shear Rate 10.0 1/s, Temperature 572 °F |
|
Solvay TECHNYL® A 218 V30 BK 34 NG PA66, 30% glass fiber, DRY Description: TECHNYL® A 218 V30 Black 34 NG is a polyamide 66, reinforced with 30% of glass fiber, heat stabilized, for injection molding. The product is available in black color.Benefits: This p.. |
|||
Viscosity | 120 cP @Shear Rate 1000 1/s, Temperature 275 °C |
120 cP @Shear Rate 1000 1/s, Temperature 527 °F |
|
Solvay TECHNYL® A 218 V30 Black 21 NHFE PA66, 30% glass fiber, DRY Description: TECHNYL® A 218 V30 BLACK 21NHFE is a polyamide 6.6, high flow, reinforced with 30% of glass fiber, heat stabilized, for injection molding. This product is available in black color.Be.. |
|||
Viscosity | 120 cP @Shear Rate 10.0 1/s, Temperature 300 °C |
120 cP @Shear Rate 10.0 1/s, Temperature 572 °F |
|
Solvay TECHNYL® A 218 V30 PA66, 30% glass fiber, DRY Description: TECHNYL® A 218 V30 is a polyamide 66, reinforced with 30% of glass fiber, heat stabilized, for injection molding. This product is available in natural and black colors.Benefits: The .. |
|||
Viscosity | 120 cP @Shear Rate 10.0 1/s, Temperature 300 °C |
120 cP @Shear Rate 10.0 1/s, Temperature 572 °F |
|
Solvay TECHNYL® A 218 V35 PA66, 35% glass fiber, DRY Description: TECHNYL® A 218 V35 is a polyamide 66, reinforced with 35% of glass fiber, heat stabilized, for injection molding. This product is available in natural and black colors.Benefits: The .. |
|||
Viscosity | 120 cP @Shear Rate 100 1/s, Temperature 280 °C |
120 cP @Shear Rate 100 1/s, Temperature 536 °F |
|
Solvay TECHNYL® A 30 H1 V30 PA66, 30% glass fiber, DRY Description: TECHNYL® A 30H1 V30 is a brominated flame retardant polyamide 66, reinforced with 30% of glass fiber, for injection molding. This product is available in natural & black color.Benefi.. |
|||
Viscosity | 120 cP @Shear Rate 10.0 1/s, Temperature 270 °C |
120 cP @Shear Rate 10.0 1/s, Temperature 518 °F |
|
Solvay TECHNYL® B 50 H1 PA66/6, DRY Description: TECHNYL® B 50H1 is an unreinforced melamine cyanurate flame retarded copolyamide 66/6. This product has been heat stabilized and is suitable for injection molding. This product is av.. |
|||
Viscosity | 120 cP @Shear Rate 1000 1/s, Temperature 250 °C |
120 cP @Shear Rate 1000 1/s, Temperature 482 °F |
|
Solvay TECHNYLSTARâ„¢ S 60G1 V30 PA6, 30% glass filled, DRY Description: TECHNYLSTARâ„¢ S 60G1 V30 is a reinforced 30% GF organophosphorous flame retarded grade based on a patented high flow polyamide 6 resin (TechnylStar). This product is heat stabilized.. |
|||
Viscosity | 120 cP @Shear Rate 100 1/s, Temperature 270 °C |
120 cP @Shear Rate 100 1/s, Temperature 518 °F |
|
Solvay TECHNYLSTARâ„¢ S 60G1 V30 PA6, 30% glass filled, DRY Description: TECHNYLSTARâ„¢ S 60G1 V30 is a reinforced 30% GF organophosphorous flame retarded grade based on a patented high flow polyamide 6 resin (TechnylStar). This product is heat stabilized.. |
|||
Viscosity | 120 cP @Shear Rate 100 1/s, Temperature 280 °C |
120 cP @Shear Rate 100 1/s, Temperature 536 °F |
|
Solvay TECHNYL® A 218 MZ15 V 25 PA66, 25/15% glass/mineral fiber, Conditioned Description: TECHNYL® A 218 MZ15 V25 is a polyamide 66, reinforced with 25% of glass fiber and 15% of mineral filler, heat stabilized, for injection molding. This product is available in black co.. |
|||
Viscosity | 120 cP @Shear Rate 100 1/s, Temperature 290 °C |
120 cP @Shear Rate 100 1/s, Temperature 554 °F |
|
Solvay TECHNYL® A 218W V30 Natural PA66, 30% glass fiber, DRY Description: TECHNYL® A 218W V30 Nat is a polyamide 66, reinforced with 30% of glass fiber, heat stabilized, for injection molding. This product is available in natural color.Benefits: The produc.. |
|||
Viscosity | 120 cP @Shear Rate 100 1/s, Temperature 280 °C |
120 cP @Shear Rate 100 1/s, Temperature 536 °F |
|
Solvay TECHNYL® A 205F PA66, DRY Description: TECHNYL ® A 205F is an unreinforced polyamide 66 for injection molding. It is available in natural color.Benefits: The product offers two main advantages: excellent filling qualities.. |
|||
Viscosity | 120 cP @Shear Rate 100 1/s, Temperature 290 °C |
120 cP @Shear Rate 100 1/s, Temperature 554 °F |
|
Solvay TECHNYL® A 205F PA66, DRY Description: TECHNYL ® A 205F is an unreinforced polyamide 66 for injection molding. It is available in natural color.Benefits: The product offers two main advantages: excellent filling qualities.. |
|||
Viscosity | 120 cP @Temperature 110 °C |
120 cP @Temperature 230 °F |
1 Hour |
Hexcel® HexFlow® RTM651 One-part Modified BMI Resin HexFlow® RTM651 is a one-component modified bismaleimide for resin transfer molding (RTM). Upon heating to 212-248°F, the resin will become a low viscosity homogeneous liquid that has a long pot-l.. |
|||
Viscosity | 120 cP @Temperature 100 °C |
120 cP @Temperature 212 °F |
|
Abatron AboCast 8708-10 One-Component Structural/Dielectric Epoxy AboCast 8708-10 is a highly filled, class H (180°C) structural, castable adhesive compound for FAST high-temperature curing. Suggested Uses: Structural bonding; Casting; Potting; Encapsulating; Em.. |
|||
Viscosity | 120 cP @Temperature 100 °C |
120 cP @Temperature 212 °F |
|
Abatron AboCast 8708-6 One-Component Structural/Dielectric Epoxy AboCast 8708-6 is a highly filled, class H (180°C) structural, castable adhesive compound for SLOW high-temperature curing. Suggested Uses: Structural bonding; Casting; Potting; Encapsulating; Emb.. |
|||
Viscosity | 120 cP @Temperature 100 °C |
120 cP @Temperature 212 °F |
|
Abatron AboCast 8708-9 One-Component Structural/Dielectric Epoxy AboCast 8708-9 is a highly filled, class H (180°C) structural, castable adhesive compound for FASTER high-temperature curing. Suggested Uses: Structural bonding; Casting; Potting; Encapsulating; E.. |
|||
Viscosity | 120 cP @Shear Rate 10.0 1/s, Temperature 280 °C |
120 cP @Shear Rate 10.0 1/s, Temperature 536 °F |
shear rate: 10/s |
Solvay TECHNYL® A 218 PA66, 33% glass fiber, DRY Standard viscosity, heat stabilized for injection molding. It is available in natural and black colors.Benefits: This product offers all the primary properties of unreinforced polyamide 66. In addit.. |