Physical Properties Metric English Comments
Viscosity 110000 - 125000 cP

@Temperature 25.0 °C
110000 - 125000 cP

@Temperature 77.0 °F
at 2.5 rpm vibration
Permabond TA4590 Toughened Acrylic Adhesive
Permabond TA4590 is a structural acrylic adhesive designed primarily for bonding metals, ferrites, ceramics and some thermoplastics. This product was specifically designed to be non-corrosive to sen..