Polymer Property : Viscosity = 130000 cP Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Viscosity 130000 cP

@Shear Rate 500 1/s,
Temperature 260 °C
130000 cP

@Shear Rate 500 1/s,
Temperature 500 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® 6131 NC010 Polybutylene Terephthalate (PBT)  (Unverified Data**)
Unreinforced Low Viscosity Polybutylene Terephthalate Crastin 6131 NC010 is an unreinforced low viscosity polybutylene terephthalate resin for extrusion and injection molding.Information provided by..
Viscosity 130000 cP

@Shear Rate 500 1/s,
Temperature 300 °C
130000 cP

@Shear Rate 500 1/s,
Temperature 572 °F
ISO 11403-1 -2
DuPont Performance Polymers Rynite® 530 NC010 Polyethylene Terephthalate (PET)  (Unverified Data**)
30% Glass Reinforced Polyethylene Terephthalate Rynite 530 NC010 is a 30% glass fiber reinforced modified polyethylene terephthalate resin with an outstanding balance of strength stiffness and tough..
Viscosity 130000 cP

@Shear Rate 300 1/s,
Temperature 190 °C
130000 cP

@Shear Rate 300 1/s,
Temperature 374 °F
Apparent Dynamic Viscosity
Dow LDPE 722M Low Density Polyethylene
DOW LDPE 722M resin is a broad molecular weight distribution homopolymer designed to offer good impact strength and stress crack resistance with excellent flexibility. Typical applications include c..
Viscosity 130000 cP

@Frequency 10.0 Hz,
Temperature 307 °C
130000 cP

@Frequency 10.0 Hz,
Temperature 585 °F
Akro-Plastic Akroloy® PA GF 50 (2706) PA 6.6 & PA6I/6T Dry, 50% Glass Filled
One of the most characteristic properties of polyamide (PA 6.6) is the absorption of moisture. This essentially leads to increased toughness and elongation at break, to name the most important param..
Viscosity 130000 cP

@Shear Rate 500 1/s,
Temperature 315 °C
130000 cP

@Shear Rate 500 1/s,
Temperature 599 °F
ISO 11403-1 -2
DuPont Performance Polymers Rynite® 935 NC010 Polyethylene Terephthalate (PET)  (Unverified Data**)
35% Glass Reinforced Polyethylene Terephthalate Rynite 935 NC010 is a 35% mica/glass reinforced modified polyethylene terephthalate resin with exceptionally low warpage excellent electrical properti..