Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 132000 cP @Shear Rate 300 1/s, Temperature 190 °C |
132000 cP @Shear Rate 300 1/s, Temperature 374 °F |
Apparent Dynamic Viscosity |
Dow DOWLEX™ IP-42 High Density Polyethylene DOWLEX® IP-42 resin is an improved processing high density polyethylene resin designed for excellent flow and high impact. DOWLEX IP-42 resin is designed by optimizing the breadth and shape of the .. |