Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 1370 cP @Temperature 25.0 °C |
1370 cP @Temperature 77.0 °F |
|
BASF Pluracol® 2100 Slabstock HR Foam Polyol Description: Pluracol® 2100 polyol is a primary terminated conventional triol designed to be used in combination with Pluracol 2130 for the production of a broad range of slabstock HR foams. Plurac.. |
|||
Viscosity | 1370 cP @Temperature 25.0 °C |
1370 cP @Temperature 77.0 °F |
|
BASF Pluracol® 380 Specialty Polyol Description: Pluracol® 380 polyol is a high molecular weight, primary hydroxyl terminated triol. The combination of high molecular weight and reactivity makes Pluracol 380 useful in the preparation.. |