Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 15 - 50 cP @Time 119 sec |
15 - 50 cP @Time 0.0330 hour |
V-128-1 |
Solvay JAGUAR® 418 Surfactant Description: Nonyl Jaguar 418 is a carboxymethylhydroxypropyl guar with extremely low residue and dual cross-linking capability. When dispersed into water with agitation it will wet out and hydrate .. |
|||
Viscosity | >= 15 cP @Temperature 156 °C |
>= 15 cP @Temperature 313 °F |
|
Hexcel® HexFlow® RTM651 One-part Modified BMI Resin HexFlow® RTM651 is a one-component modified bismaleimide for resin transfer molding (RTM). Upon heating to 212-248°F, the resin will become a low viscosity homogeneous liquid that has a long pot-l.. |
|||
Viscosity | 15 cP @Temperature 210 °C |
15 cP @Temperature 410 °F |
Melt (Unpolymerized resin); Cone and plate 10 1/s shear rate |
Cyclics CBT® 100 Thermoplastic Resin CBT® 100 resin melts to a water-like viscosity when heated, then polymerizes into the engineering thermoplastic resin polybutylene terephthalate (PBT). CBT 200 resin has a processing range between.. |