Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | >= 155 cP @Time 7200 sec |
>= 155 cP @Time 2.00 hour |
V-1-4 |
Solvay JAGUAR® HP 8FF Surfactant Description: Hydroxypropyl guar with extremely low residue, designed to be easily dispersed into water where it will wet out and hydrate, forming a viscous HPG fluid which will readily crosslink wit.. |
|||
Viscosity | >= 155 cP @Time 86400 sec |
>= 155 cP @Time 24.0 hour |
V-1-4 |
Solvay JAGUAR® HP 8FF Surfactant Description: Hydroxypropyl guar with extremely low residue, designed to be easily dispersed into water where it will wet out and hydrate, forming a viscous HPG fluid which will readily crosslink wit.. |