Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 160000 cP @Shear Rate 1000 1/s, Temperature 190 °C |
160000 cP @Shear Rate 1000 1/s, Temperature 374 °F |
Apparent Dynamic Viscosity |
Dow HDPE 12450N High Density Polyethylene DOW HDPE 12450N resin is a narrow molecular weight distribution copolymer designed to offer excellent impact strength and toughness with moderate stiffness. This resin has good processability over a.. |
|||
Viscosity | 160000 cP @Frequency 10.0 Hz, Temperature 292 °C |
160000 cP @Frequency 10.0 Hz, Temperature 558 °F |
|
Akro-Plastic Akroloy® PA GF 50 (2706) PA 6.6 & PA6I/6T Dry, 50% Glass Filled One of the most characteristic properties of polyamide (PA 6.6) is the absorption of moisture. This essentially leads to increased toughness and elongation at break, to name the most important param.. |