Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 16600 cP @Temperature 25.0 °C |
16600 cP @Temperature 77.0 °F |
Part A |
Lord Adhesives Circalokâ„¢ 6009 A/B Flame Retardant Epoxy Encapsulant Circalokâ„¢ 6009 A/B is a two component epoxy resin system which has moderate thermal conductivity and low viscosity. Circalokâ„¢ 6009 A/B meets UL 94V-0 specification for flame retardance.All.. |