Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 167000 cP @Shear Rate 2000 1/s, Temperature 260 °C |
167000 cP @Shear Rate 2000 1/s, Temperature 500 °F |
ISO 11443 |
DuPont Performance Polymers Crastin® SK609 NC010 PBT
(Unverified Data**) Crastin® SK609 NC010 is a 50% glass fiber reinforced, lubricated polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Viscosity | 167000 cP @Shear Rate 500 1/s, Temperature 295 °C |
167000 cP @Shear Rate 500 1/s, Temperature 563 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 70G30HSL BK039B Nylon 66
(Unverified Data**) 30% Glass Reinforced Heat Stabilized Polyamide 66 Information provided by DuPont Performance Polymers |