Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 1000 - 1800 cP @Temperature 52.2 °C |
1000 - 1800 cP @Temperature 126 °F |
Part A |
Master Bond EP42HT-2Med Epoxy Meets USP Class VI Requirements Description: Master Bond Polymer System EP42HT-2Med is a room temperature curable two component epoxy, adhesive, sealant, coating and casting material featuring high temperature resistance along wit.. |
|||
Viscosity | 1000 - 1800 cP @Temperature 52.2 °C |
1000 - 1800 cP @Temperature 126 °F |
Part A |
Master Bond EP42HT-2 Epoxy Adhesive Resists Sterilization Description: Master Bond Polymer System EP42HT-2 is a room temperature curable, two component epoxy adhesive, sealant, coating and casting material featuring high temperature resistance along with o.. |
|||
Viscosity | 1000 - 1800 cP @Temperature 51.7 °C |
1000 - 1800 cP @Temperature 125 °F |
Part A |
Master Bond EP42HT-2FG Two Component Epoxy Adhesive for Food Applications Master Bond Polymer System EP42HT-2FG is a room temperature setting, two component epoxy adhesive, sealant and coating specially formulated for food applications. It has been independently tested an.. |
|||
Viscosity | 1000 - 1800 cP @Temperature 52.0 °C |
1000 - 1800 cP @Temperature 126 °F |
Part A |
Master Bond EP42HT-2LO Low Outgassing, Heat Resistant Two Component Epoxy Master Bond Polymer System EP42HT-2LO is a room temperature curable two component epoxy, adhesive, sealant, coating and casting material featuring high temperature resistance along with outstanding .. |