Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 192300 cP @Shear Rate 500 1/s, Temperature 240 °C |
192300 cP @Shear Rate 500 1/s, Temperature 464 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® S610SF NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**)< Unreinforced Low Viscosity Polybutylene Terephthalate Developed for Super Fast Production Crastin S610SF is an unreinforced low viscosity polybutylene terephthalate for injection molding. It has hig.. |