Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 193000 cP @Shear Rate 5000 1/s, Temperature 250 °C |
193000 cP @Shear Rate 5000 1/s, Temperature 482 °F |
ISO 11403-1 -2 |