Polymer Property : Viscosity = 2.00e+6 cP Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Viscosity 1.00e+6 - 2.00e+6 cP

@Temperature 190 - 190 °C
1.00e+6 - 2.00e+6 cP

@Temperature 374 - 374 °F
Average value: 1.24e+6 cP Grade Count:5
Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Extrusion/Coating Grade
This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Acetate Copolymer (EVA), Extrusion/Coating Grade". Each property range of values reported..
Viscosity 1.00e+6 - 2.00e+6 cP

@Shear Rate 50.0 - 50.0 1/s
1.00e+6 - 2.00e+6 cP

@Shear Rate 50.0 - 50.0 1/s
Average value: 1.24e+6 cP Grade Count:5
Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Extrusion/Coating Grade
This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Acetate Copolymer (EVA), Extrusion/Coating Grade". Each property range of values reported..
Viscosity 2.00e+6 - 2.00e+6 cP

@Temperature 190 - 190 °C
2.00e+6 - 2.00e+6 cP

@Temperature 374 - 374 °F
Average value: 2.00e+6 cP Grade Count:2
Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Film Grade
This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Acetate Copolymer (EVA), Film Grade". Each property range of values reported is minimum a..
Viscosity 2.00e+6 - 2.00e+6 cP

@Shear Rate 50.0 - 50.0 1/s
2.00e+6 - 2.00e+6 cP

@Shear Rate 50.0 - 50.0 1/s
Average value: 2.00e+6 cP Grade Count:2
Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Film Grade
This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Acetate Copolymer (EVA), Film Grade". Each property range of values reported is minimum a..
Viscosity 2.00e+6 - 2.00e+6 cP

@Temperature 240 - 240 °C
2.00e+6 - 2.00e+6 cP

@Temperature 464 - 464 °F
Average value: 2.00e+6 cP Grade Count:1
Overview of materials for Acrylic, Optical Grade, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Optical Grade, Molded". Each property range of values reported is minimum and maximum values of..
Viscosity 2.00e+6 - 2.00e+6 cP

@Shear Rate 100 - 100 1/s
2.00e+6 - 2.00e+6 cP

@Shear Rate 100 - 100 1/s
Average value: 2.00e+6 cP Grade Count:1
Overview of materials for Acrylic, Optical Grade, Molded