Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 20.0 - 500 cP @Temperature 270 - 300 °C |
20.0 - 500 cP @Temperature 518 - 572 °F |
Average value: 141 cP Grade Count:8 |
Overview of materials for Nylon 66, 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% are included. .. |
|||
Viscosity | 20.0 - 500 cP @Shear Rate 10.0 - 1000 1/s |
20.0 - 500 cP @Shear Rate 10.0 - 1000 1/s |
Average value: 141 cP Grade Count:8 |
Overview of materials for Nylon 66, 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% are included. .. |
|||
Viscosity | 20.0 - 300 cP @Temperature 275 - 300 °C |
20.0 - 300 cP @Temperature 527 - 572 °F |
Average value: 144 cP Grade Count:2 |
Overview of materials for Nylon 66, 40% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 40% Glass Fiber Filled". Specific grades with glass content between 35% and 44% are included. .. |
|||
Viscosity | 20.0 - 300 cP @Shear Rate 10.0 - 1000 1/s |
20.0 - 300 cP @Shear Rate 10.0 - 1000 1/s |
Average value: 144 cP Grade Count:2 |
Overview of materials for Nylon 66, 40% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 40% Glass Fiber Filled". Specific grades with glass content between 35% and 44% are included. .. |
|||
Viscosity | 20.0 - 450 cP @Temperature 280 - 300 °C |
20.0 - 450 cP @Temperature 536 - 572 °F |
Average value: 47200 cP Grade Count:1 |
Overview of materials for Nylon 66, 50% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 50% Glass Fiber Filled". Specific grades with glass content between 45% and 54% are included. .. |
|||
Viscosity | 20.0 - 450 cP @Shear Rate 10.0 - 1000 1/s |
20.0 - 450 cP @Shear Rate 10.0 - 1000 1/s |
Average value: 47200 cP Grade Count:1 |
Overview of materials for Nylon 66, 50% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 50% Glass Fiber Filled". Specific grades with glass content between 45% and 54% are included. .. |