Polymer Property : Viscosity = 243400 cP Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Viscosity 243400 cP

@Shear Rate 5000 1/s,
Temperature 260 °C
243400 cP

@Shear Rate 5000 1/s,
Temperature 500 °F
ISO 11403-1 -2
DuPont Performance Polymers Zytel® FR70G25V0 NC010 Nylon 66  (Unverified Data**)
25% Glass Reinforced Flame Retardant Polyamide 66 Zytel FR70G25V0 NC010 is a 25% glass fiber reinforced heat stabilized flame retardant polyamide 66 resin for injection molding.Information provided ..