Physical Properties Metric English Comments
Viscosity 265000 cP

@Shear Rate 300 1/s,
Temperature 190 °C
265000 cP

@Shear Rate 300 1/s,
Temperature 374 °F
Apparent Dynamic Viscosity
Dow LDPE 640IM Low Density Polyethylene
DOW LDPE 640IM resin is a broad molecular weight distribution homopolymer designed to offer excellent impact strength and stress crack resistance with moderate stiffness for general purpose, and cap..
Viscosity 265000 cP

@Shear Rate 500 1/s,
Temperature 260 °C
265000 cP

@Shear Rate 500 1/s,
Temperature 500 °F
ISO 11403-1 -2
DuPont Performance Polymers Sorona® 3030G NC010 Polytrimethylene Terephthalate (PTT)  (Unverified Data**)&
30% Glass Reinforced Polytrimethylene Terephthalate Sorona 3030G NC010 is a 30% glass reinforced PTT resin containing 25% renewably sourced ingredients by weight (37% based on polymer only) with goo..