Physical Properties Metric English Comments
Viscosity 27000 cP

@Shear Rate 1340 1/s,
Temperature 200 °C
27000 cP

@Shear Rate 1340 1/s,
Temperature 392 °F
ASTM D3835
PolyOne Dynalloy™ 8900-30 Thermoplastic Elastomer (TPE)
Dynalloy™ 8900-series is an innovative thermoplastic elastomer selection formulated to provide the injection molder with a product capable of overmolding and bonding to both low-density polyethylen..
Viscosity 27000 cP

@Shear Rate 11200 1/s,
Temperature 200 °C
27000 cP

@Shear Rate 11200 1/s,
Temperature 392 °F
ASTM D3835
PolyOne Dynalloy™ OBC 8100-N65 Thermoplastic Elastomer (TPE)
Dynalloy™ OBC8100-N65 is a TPE developed utilizing the unique rubber properties of Dow INFUSE™ Olefin Block Copolymers. The 8100 Series has been specifically developed for applications requiring t..
Viscosity 27000 cP

@Shear Rate 11200 1/s,
Temperature 200 °C
27000 cP

@Shear Rate 11200 1/s,
Temperature 392 °F
ASTM D3835
PolyOne Dynalloy™ OBC8200-BT50 Thermoplastic Elastomer (TPE)
Dynalloy™ OBC8200-BT50 is a translucent grade to be used in blow molding applications. New Product. Commercial specifications have not been established. - Excellent Colorability - Rubbery FeelPurge..
Viscosity 27000 cP

@Shear Rate 5000 1/s,
Temperature 190 °C
27000 cP

@Shear Rate 5000 1/s,
Temperature 374 °F
Apparent Dynamic Viscosity
Dow DOWLEX™ 2503.10 Linear Low Density Polyethylene, Narrow MW Distribution
DOWLEX® 2503.10 Polyethylene resin is a narrow molecular weight distribution copolymer designed as a superior processing resin. For very thin wall higher cavitation molding, this grade often is a p..
Viscosity 27000 cP

@Shear Rate 5000 1/s,
Temperature 190 °C
27000 cP

@Shear Rate 5000 1/s,
Temperature 374 °F
Apparent Dynamic Viscosity
Dow LDPE 955I Low Density Polyethylene
DOW LDPE 955I resin is a medium molecular weight distribution homo polymer designed to offer excellent clarity and flexibility, and good toughness, with low warpage. Typical applications include lid..