Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 28000 cP @Shear Rate 5000 1/s, Temperature 190 °C |
28000 cP @Shear Rate 5000 1/s, Temperature 374 °F |
Apparent Dynamic Viscosity |
Dow LDPE 993I Low Density Polyethylene DOW LDPE 993I resin is a low slip, medium molecular weight distribution homopolymer designed to offer good gloss and rigidity with excellent flow characteristics. This resin has good processability .. |