Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 282300 cP @Shear Rate 500 1/s, Temperature 250 °C |
282300 cP @Shear Rate 500 1/s, Temperature 482 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 6356 Polyester Elastomer TPC-ET
(Unverified Data**) 63 Shore D High Performance Polyester ElastomerInformation provided by DuPont Performance Polymers |