Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 3.2 cP @Temperature 93.3 °C |
3.2 cP @Temperature 200 °F |
|
Paratherm Corporation Paratherm™ GLT™ Heat Transfer Fluid Paratherm GLT™ Heat Transfer Fluid is an alkylated aromatic based heat transfer fluid formulated for closed loop liquid phase heating systems to 550°F using fired heaters and to 575°F in waste-he.. |
|||
Viscosity | 3.2 cP @Temperature 100 °C |
3.2 cP @Temperature 212 °F |
|
Teknor Apex TruVis Esters™ DINA Di-Isononyl Adipate |