Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 3000 cP @Temperature 40.0 °C |
3000 cP @Temperature 104 °F |
|
BASF Pluracol® 1578 Rigid Polyol Description: Pluracol® 1578 polyol is a general purpose aromatic initiator-based polyol for rigid foams for use in a variety of applications. It is attractively priced for consideration for foaming.. |
|||
Viscosity | 3000 cP @Temperature 45.0 °C |
3000 cP @Temperature 113 °F |
|
Lendell Manufacturing Prepol Pre Polymer Liquid Apperance, Amber, honey likePolyether Polyurethane Pre-Polymer is water activated, yielding foams and gels with unique characteristics - Hydrophilic, Bio-Compatible, loading of additives to 8.. |