Physical Properties Metric English Comments
Viscosity 305000 cP

@Shear Rate 300 1/s,
Temperature 190 °C
305000 cP

@Shear Rate 300 1/s,
Temperature 374 °F
Apparent Dynamic Viscosity
Dow LDPE 510I Low Density Polyethylene
DOW LDPE 510I resin is a broad molecular weight distribution homopolymer designed to offer excellent impact strength and stress crack resistance with moderate flexibility, for caps/closures, etc. It..