Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 35755 cP @Shear Rate 5000 1/s, Temperature 290 °C |
35755 cP @Shear Rate 5000 1/s, Temperature 554 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® FE5382 BK276 Nylon 612
(Unverified Data**) 33% Glass Reinforced Polyamide 612 Developed for Electrical and Electronics Applications Zytel FE5382 BK276 is a 33% glass fiber reinforced heat stabilized black polyamide 612 resin developed for el.. |