Viscosity 40 cP

@Temperature 25.0 °C
40 cP

@Temperature 77.0 °F
Uncured
Permabond 931 Cyanoacrylate
PERMABOND 931 is a low odor, non­fogging, non­frosting cyanoacrylate. The reduced odor improves worker comfort. Unsightly fogging adjacent to bondlines, common with other cyanoacrylate adhesiv..
Viscosity 40 cP

@Temperature 25.0 °C
40 cP

@Temperature 77.0 °F
Part B
Lord Adhesives Circalokâ„¢ 6009 A/B Flame Retardant Epoxy Encapsulant
Circalokâ„¢ 6009 A/B is a two component epoxy resin system which has moderate thermal conductivity and low viscosity. Circalokâ„¢ 6009 A/B meets UL 94V-0 specification for flame retardance.All..