Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 416000 cP @Shear Rate 500 1/s, Temperature 200 °C |
416000 cP @Shear Rate 500 1/s, Temperature 392 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 525GR NC000 Acetal (POM)
(Unverified Data**) 25% Glass Reinforced Medium Viscosity Acetal Homopolymer Delrin 525GR NC000 is a 25% glass reinforced acetal homopolymer for injection molding. It has very high strength stiffness and high deflectio.. |