Polymer Property : Viscosity = 421400 cP Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Viscosity 421400 cP

@Shear Rate 500 1/s,
Temperature 215 °C
421400 cP

@Shear Rate 500 1/s,
Temperature 419 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® 300PE BK602 Acetal (POM)  (Unverified Data**)
Medium-high Viscosity Acetal Homopolymer with Very Low Emissions Delrin 300PE BK602 (formerly DE20577) is a medium-high viscosity acetal homopolymer an enhanced version of Delrin 300CP with very low..