Physical Properties Metric English Comments
Viscosity 45000 cP

@Temperature -40.0 °C
45000 cP

@Temperature -40.0 °F
ExxonMobil Mobil ATF Type F
Mobil ATF Type F is an automatic transmission fluid which is made from high quality base oils with viscosity index improvers, antioxidants, anti-wear agents, defoamants and special additives to prov..
Viscosity 45000 cP

@Shear Rate 5000 1/s,
Temperature 190 °C
45000 cP

@Shear Rate 5000 1/s,
Temperature 374 °F
Apparent Dynamic Viscosity
Dow LDPE 5004IM Low Density Polyethylene
DOW LDPE 5004IM resin is a broad molecular weight distribution homopolymer designed to offer good impact strength and rigidity with high ESCR. This resin has good processability over a wide range of..
Viscosity 45000 cP

@Temperature -40.0 °C
45000 cP

@Temperature -40.0 °F
ExxonMobil Mobil ATF Type F
Mobil ATF Type F is an automatic transmission fluid which is made from high quality base oils with viscosity index improvers, antioxidants, anti-wear agents, defoamants and special additives to prov..