Physical Properties Metric English Comments
Viscosity 473000 - 473000 cP

@Temperature 177 - 177 °C
473000 - 473000 cP

@Temperature 351 - 351 °F
Average value: 473000 cP Grade Count:1
Overview of materials for PVC, Flexible Grade
This property data is a summary of similar materials in the MatWeb database for the category "PVC, Flexible Grade". Each property range of values reported is minimum and maximum values of appropriat..
Viscosity 473000 - 473000 cP

@Frequency 1000 - 1000 Hz
473000 - 473000 cP

@Frequency 1000 - 1000 Hz
Average value: 473000 cP Grade Count:1
Overview of materials for PVC, Flexible Grade
This property data is a summary of similar materials in the MatWeb database for the category "PVC, Flexible Grade". Each property range of values reported is minimum and maximum values of appropriat..