Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 57000 cP @Shear Rate 5000 1/s, Temperature 315 °C |
57000 cP @Shear Rate 5000 1/s, Temperature 599 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Rynite® 415HP NC010 Polyethylene Terephthalate (PET)
(Unverified Data**) 15% Glass Reinforced Polyethylene Terephthalate with Excellent Impact Resistance Rynite 415HP NC010 is a 15% glass reinforced modified polyethylene terephthalate improved for easy fast processing ov.. |
|||
Viscosity | 57000 cP @Shear Rate 5000 1/s, Temperature 295 °C |
57000 cP @Shear Rate 5000 1/s, Temperature 563 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Rynite® 935 NC010 Polyethylene Terephthalate (PET)
(Unverified Data**) 35% Glass Reinforced Polyethylene Terephthalate Rynite 935 NC010 is a 35% mica/glass reinforced modified polyethylene terephthalate resin with exceptionally low warpage excellent electrical properti.. |