Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 61310 cP @Shear Rate 5000 1/s, Temperature 245 °C |
61310 cP @Shear Rate 5000 1/s, Temperature 473 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® G5544 Polyester Elastomer TPC-ET
(Unverified Data**) 55 Shore D Standard Performance Polyester Elastomer with Heat Ageing ProtectionHytrel G5544 is a medium modulus grade with nominal hardness of 55D. It contains discoloring stabilizer. It can be proc.. |
|||
Viscosity | 61310 cP @Shear Rate 5000 1/s, Temperature 280 °C |
61310 cP @Shear Rate 5000 1/s, Temperature 536 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 101L NC010 Nylon 66
(Unverified Data**) Unreinforced Polyamide 66Zytel 101L NC010 is a lubricated polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |