Polymer Property : Viscosity = 7.7 cP
Polymer Property :
Viscosity =
7.7 cP
Product List
Physical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties
Metric
English
Comments
Viscosity
7.7
cP
@Temperature 100 °C
7.7
cP
@Temperature 212 °F
Teknor Apex TruVis Esters™ 810TM N-C8C10 Trimellitate