Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 7.73e+6 cP @Shear Rate 1.58 1/s, Temperature 190 °C |
7.73e+6 cP @Shear Rate 1.58 1/s, Temperature 374 °F |
1.58 rad/sec; ARES Rheometer |
Dow Engage® ENR 7270.00 Ethylene-Butene Copolymer Description: ENR 7270.00 is a general purpose ethylene-butene copolymer designed to provide good cost/performance balance in polymer modification applications.Information provided by manufacturer.Th.. |