Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 7060 cP @Temperature -15.0 °C |
7060 cP @Temperature 5.00 °F |
Cold Cranking Simulator (CCS); ASTM D5293 |
ExxonMobil 20W-50 Exxon Aviation Oil Elite Aviation Oil 20W-50 is a premium quality, semi-synthetic, ashless-dispersant aviation piston engine oil. It is formulated from select, highly refined mineral base oils, a polyalphaolefin synthetic .. |
|||
Viscosity | 7060 cP @Temperature -15.0 °C |
7060 cP @Temperature 5.00 °F |
Cold Cranking Simulator (CCS); ASTM D5293 |
ExxonMobil 20W-50 Exxon Aviation Oil Elite Aviation Oil 20W-50 is a premium quality, semi-synthetic, ashless-dispersant aviation piston engine oil. It is formulated from select, highly refined mineral base oils, a polyalphaolefin synthetic .. |