Viscosity 76000 cP

@Shear Rate 5000 1/s,
Temperature 190 °C
76000 cP

@Shear Rate 5000 1/s,
Temperature 374 °F
Apparent Dynamic Viscosity
Dow LDPE 510I Low Density Polyethylene
DOW LDPE 510I resin is a broad molecular weight distribution homopolymer designed to offer excellent impact strength and stress crack resistance with moderate flexibility, for caps/closures, etc. It..
Viscosity 76000 cP

@Shear Rate 1000 1/s,
Temperature 190 °C
76000 cP

@Shear Rate 1000 1/s,
Temperature 374 °F
Apparent Dynamic Viscosity
Dow LDPE 722M Low Density Polyethylene
DOW LDPE 722M resin is a broad molecular weight distribution homopolymer designed to offer good impact strength and stress crack resistance with excellent flexibility. Typical applications include c..
Viscosity 76000 cP

@Shear Rate 300 1/s,
Temperature 190 °C
76000 cP

@Shear Rate 300 1/s,
Temperature 374 °F
Apparent Dynamic Viscosity
Dow LDPE 993I Low Density Polyethylene
DOW LDPE 993I resin is a low slip, medium molecular weight distribution homopolymer designed to offer good gloss and rigidity with excellent flow characteristics. This resin has good processability ..