Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 779300 cP @Shear Rate 500 1/s, Temperature 215 °C |
779300 cP @Shear Rate 500 1/s, Temperature 419 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 100PE NC010 Acetal (POM)
(Unverified Data**) High Viscosity Acetal Homopolymer with Very Low Emissions Delrin 100PE NC010 (formerly DE20573) is a high viscosity acetal homopolymer an enhanced version of Delrin 100P with very low VOC emissions... |