Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Viscosity 84000 cP

@Shear Rate 5000 1/s,
Temperature 230 °C
84000 cP

@Shear Rate 5000 1/s,
Temperature 446 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® 525GR NC000 Acetal (POM)  (Unverified Data**)
25% Glass Reinforced Medium Viscosity Acetal Homopolymer Delrin 525GR NC000 is a 25% glass reinforced acetal homopolymer for injection molding. It has very high strength stiffness and high deflectio..
Viscosity 84000 cP

@Shear Rate 5000 1/s,
Temperature 230 °C
84000 cP

@Shear Rate 5000 1/s,
Temperature 446 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® 527UV NC010 Acetal (POM)  (Unverified Data**)
UV Stabilized Medium Viscosity Acetal HomopolymerDelrin 527UV NC010 is a medium viscosity acetal homopolymer resin with UV stabilizers developed for automotive interior applications. It has improvem..